Abstract

A new electrolytic method was developed to prepare LiCo_(x)Ni_(1-x)O_2 as a cathode material of lithium-ion battery. Contrary to the traditional method, electrolytic method is a potential method with simple process to industrialization and no pollution. Metal cobalt and nickel were electrolysed in parallel to prepare the precursor of Co_( x )Ni_(1- x )(OH)_2.Different compositional precursors could be conveniently prepared by changing electrolytic current. The LiCo_(0.3)Ni_(0.7)O_2 cathode prepared by this method was found favorable charge-discharge and cycle properties. For the LiCo_(0.3)Ni_(0.7)O_(2 )cathode material, the discharge capacities in the 1st and 50th cycles were 163 mAh/g and 140 mAh/g with charge retention of 86%.

Keywords

Lithium ion battery, Cathode material, LiCo_(x)Ni_(1-x)O_(2, )Electrolysis

Publication Date

2004-11-28

Online Available Date

2004-11-28

Revised Date

2004-11-28

Received Date

2004-11-28

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.