Abstract

The storage performance of nickel-metal-hydride (Ni-MH) battery was studied by using galvanostatic charge-discharge and cyclic voltammetry. The experimental results indicated that CoOOH could not be completely restored after its being thoroughly reduced at lower potential, which might weaken electric conduction network in the positive electrode and result in fading of electrochemical properties of Ni-MH battery. Addition of nickel powder as a conductive agent into the positive electrode was beneficial to the capacity recovery after storage.

Keywords

Nickel-metal-hydride battery, Storage performance, Electric conduction network, Nickel powder

Publication Date

2004-11-28

Online Available Date

2004-11-28

Revised Date

2004-11-28

Received Date

2004-11-28

References

[1] OshitaniM,YufuH,TakashimaK,etal.Developmentofapastednickelelectrodewithhighactivematerialutilization[J].J.Electrochem.Soc.,1989,136:1590~1593.
[2] VaidyanathanH.Long termstorageofnickel hydrogencells[J].J.PowerSources,1988,22:221~228.
[3] AravamuthanS,AnnammaCV,PillaiNR,etal.Studiesonthestorageofelectrochemicallyimpregnatednickel/cadmiumcells[J].J.PowerSources,1994,50:81~87.
[4] JimHS,StadnickSJ.Effectofprechargeonnickel hydrogenbatterystoragecapacity[J].J.PowerSources,1989,27:69~79.
[5] BerndtD.Maintenance freeBattery,AHandbookofBatteryTechnology[M].Taunton,Somerset,UK:ResearchStudiesPress:1993.207,212~213.
[6] JIJin.AstudyonthestorageperformanceofMH/Nicells[J].BatteryBimonthly,2000,30:219~220.

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.