Corresponding Author

Dan_hong CHENG

Abstract

Recent progress in the research on composite coatings prepared by electroplating technology is reviewed. The nanoscaled particles, electrocatalytic, photoactive composite coatings are emphatically discussed. The composite coatings prepared by dispersing nanoscaled particles could attain better hardness, wear resistance and corrosion resistance than those of composite coatings which prepared by adding micronscaled particles. As compared with pure metal electrode and alloy electrode, some electrocatalytic composite coatings electrode could markedly reduce the overvoltages of cathodic and anodic electrode reaction. In recent years, the electrocatalytic composite coatings which based on metal oxides and conductive polymer as matrix materials become a newest field of composite electroplating technology.

Publication Date

2003-05-28

Online Available Date

2003-05-28

Revised Date

2003-05-28

Received Date

2003-05-28

References

[1] GuoHe_tong,ZhangSan_yuan.CompositeCoatings[M].Tianjin:TianjinUniversityPress,1991,123~129.

[2] GuoZhong_cheng,ZhuXiao_yun,ZhengYan_ping,etal.StudyoncorrosionresistanceofelectrodepositedRE_Ni_W_P_SiC[J].Mater.Prop.,2000,33(2):329.

[3] SapuGN,RameshKR,ThiruchelvamT.Validityofadsorptionmechanismforelectrodepositedzinccomposites[J].BulletinofElectrochemistry,2001,17(9):405~408.

[4] GuoZhong_cheng,DengGuan_hao,YangXian_wan,etal.WearresistanceofelectrodepositedRE_Ni_W_P_SiC_PTFEcompositecoating[J].MaterialProtection(材料保护),2001,34(1):4~11.

[5] MusianiM.Electrodepositionofcomposites:anexpandingsubjectinelectrchemicalmaterialsscience[J].Electrochim.Acta,2000,45:3397.

[6] HiratoT,FransaerJ,CelisJP.ElectrolyticcodepositionofsilicaparticleswithaluminumfromAlCl3_dmethylsulfoneelectrolytes[J].J.Electrochem.Soc.,2001,148(4):C280.

[7] LeeWun_hsing,TangSen_chen,ChungKung_cheng.Effectsofdirectcurrentandpulse_platingonco_depositionofnickelandnanometerdiamondpowder[J].SurfaceandCoatingsTechnology,1999,120~121:607.

[8] VidrineAB,PodlahaEJ.Compositeelectrodepositionofultrafineγ_aluminaparticlesinnickelmatricesPartI:Citrateandchlorideelectrolytes[J].J.App1.Electrochem.,2001,31:461.

[9] 0rlovskajaL,PerieneN,KurtinaitieneM,etal.Ni_SiCcompositeplatedunderamodulatedcurrent[J].SurfaceandCoatingsTechnology,1999,111:234.

[10] SteinbachJ,FerkelH.NanaostructuredNi_Al2O3filmspreparedbyD.C.andpulsedD.C.electroplating[J].ScriptaMater.,2001,44:1813.

[11] MandichNV,DennisJK.Codepositionofnanodiamondswithchromium[J].MetalFinishing,2001,99(6):117.

[12] BeneaL,BonoraPL,BorelloA,etal.Wearcorrosionpropertiesofnano_structuredSiC_nickelcompositecoatingsobtainedbyelectroplating[J].Wear,2002,249:995.

[13] DeguchiT,ImaiK,MatsuiH,etal.RapidelectroplatingofphotocatalyticallyhighlyactiveTiO2_Znnanocompositefilmsonsteel[J].Mater.Sci.,2001,36:4723.

[14] MollerA,HahnH.SynthesisandcharacterizationofnanocrystalineNi/ZrO2compositecoating[J].NanostructuredMaterials,1999,12:259.

[15] StojakJL,TalbotJB.Effectofparticlesonpolarizationduringelectrodepositionusingarotatingcylinderelelctrode[J].J.Appl.Electrochem.,2001,31:559.

[16] PetrovaM,KupperM,LoweH,etal.Electrodepositednickeldispersioncoatingswithhardnano_sizeparticlesformicrotechnologyapplication[J].Galvanotechnik,2001,92(5):1366(inGerman,CA,Vol135:217565d).

[17] YuJing_ku,ZhaoYu_cheng,GaoYu_Wei,etal.Compositebrush_platingNi_diamondcoating[J].DiamondandMould,WearMaterial(金刚石与磨料磨具工程),2001,2(122):7.

[18] MullerB,FerkelH.Al2O3_nanoparticledistributioninplatednickelcompositefilms[J].NanostructuredMaterials,1998,10(8):1285.

[19] FerkelH,MullerB,RiehemannW,etal.Electrodepositionofparticle_strengthenednickelfilms[J].MaterialsScienceandEngineeringA,1997,234_236:474.

[20] JeongDH,GonzalezF,PalumboG,etal.Theeffectofgrainsizeonthewearpropertiesofelectrodepositednanocrystallinenickelcoatings[J].ScriptaMater.,2001,44:493.

[21] GyttouP,PavlatoEA,SpyellisN,etal.HardeningmodificationofnickelmatrixcompositeelectrocoatingscontainingSiCnanoparticles[J].Electroplating&SurfaceTreatment,2001.9(1):23~28.

[22] ChenXH,DengFM,LuXN,etal.Carbonnanotubes_Nicompositecoatingwithhigh_wearability[C] .Beijing:3rdInternationalSymposiumonTribo_Fatigue,2000.

[23] WangJiang_xiong,ChengXiao_hua,PengJing_cui,etal.ApreliminaryinvestigationofthecorrosionresistanceofNi_carbonnanotubescompositecoating[J].Corrosion&Protection(腐蚀与防护),2002,23(1):6.

[24] BurkatGK,DolmatovVYu.Electrodepositionandpropertiesofzinc_diamondcoatingsobtainedinzincatesolutions[J].Electroplating&SurfaceTreatment,2001.9(2):35.

[25] KunugiY,FuchigamiT,NonakaT,etal.Electrolysisusingcomposite_platedelectrodePartⅡ.Electrooxidationofalcoholsatahydrophobicnickel/poly(terafluoroethylene)composite_platedanode[J].J.Electroanal.Chem.,1990,287:385.

[26] KunugiY,KumadaR,NonakaT,etal.Electrolysisusingcomposite_platedelectrodePartⅢ.Electroorganicreactionsonahydrophobicnickel/PTFEcomposite_platednickelelectrode[J].J.Electroanal.Chem.,1991,313:215.

[27] KunugiY.NonakaT,ChongYB,et

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.